Submitted by hotspicynoodles t3_104ldbr in MachineLearning
KBM_KBM t1_j35r12q wrote
Do you have target labels for how much defect do you have against the flow?
hotspicynoodles OP t1_j35txz9 wrote
The data consists of flowrate and defect column, if there is no defect for eg. flow doesn't go above 8 lpm, then there is no default. If it does exceed then "Porosity" is mentioned with that flow rate.
Anjum48 t1_j38bc0o wrote
Does the data include the type of material being welded (and possibly thickness)? I think certain metals e.g. titanium, stainless, etc. may need different torch cups and therefore different flow rates